Recovery of noble metals from floor sweeping jewelry waste ...
· Experimental results demonstrated that the flotation method was very successful in diminishing much of the waste fraction. A froth product, with more than 280 g/t Au and 2800 g/t Ag, was produced from a feed containing 174 g/t Au and 1834 g/t Ag with approximately 87% Au and 82% Ag recoveries. To investigate the dissolution behaviors of gold and silver, cyanide leaching tests were .