After agglomeration, the mineral bearing ore was dried on a 10 mesh sieve for 24 hours at 20° C. and 50% relative humidity. After drying, the samples were subjected to submersion/dispersion testing. The submersion/dispersion testing measures the weight of fines washed from the agglomerates after a 3 minute submersion.